1/31/2022 | 3816000000 | REFRACTORY CONCRETE BASED ON BOXITE WITH LOW IRON CONTENT, SUPPLIED DRY, BOUND TYPE HYDRAULIC, CHEMICAL COMPOSITION AL2O3 52-56%, SIO2 25-29%, SIC 5-9%, ZRO2 4-8%, FE2O3 LESS THAN 1.5 %. MAXIMUM APPLICATION TEMPERATURE 1500░C. FAST | 20000 | 26674.9 | Spain | GORNAL SPAIN | BRANCH OF HAYDELBERGCEMENT RUS LLC ON ORDER OF HAYDELBERGCEMENT RUS LLC |
1/31/2022 | 3816000000 | REFRACTORY CONCRETE BASED ON BOXITE WITH LOW IRON CONTENT, SUPPLIED DRY, BOUND TYPE HYDRAULIC, CHEMICAL COMPOSITION AL2O3 52-56%, SIO2 25-29%, SIC 5-9%, ZRO2 4-8%, FE2O3 LESS THAN 1.5 %. MAXIMUM APPLICATION TEMPERATURE 1500░C. FAST | 13000 | 17339.5 | Spain | GORNAL SPAIN | BRANCH OF HAYDELBERGCEMENT RUS LLC ON ORDER OF HAYDELBERGCEMENT RUS LLC |
1/25/2022 | 3824400000 | ACCELERATOR OF SETTING (HARDENING) OF CEMENT MORTAR OF CONCRETE, THE MAIN COMPONENTS ARE: ALUMINUM SULFATE, ALUMINUM OXIDE, IRON SULFATE, IRON OXIDE PRODUCED IN RATIO 3:0.5:2:1. ON THE APPEARANCE WHITE (OR GRAY, BROWN), | 20000 | 14817.5 | China | Kyzyl | LUNSIN LLC |
1/25/2022 | 3824400000 | ACCELERATOR OF SETTING (HARDENING) OF CEMENT MORTAR OF CONCRETE, THE MAIN COMPONENTS ARE: ALUMINUM SULFATE, ALUMINUM OXIDE, IRON SULFATE, IRON OXIDE OBTAINED IN RATIO 3:0.5:2:1. | 20000 | 14817.5 | China | Kyzyl | LUNSIN LLC |
1/31/2022 | 3816000000 | FIREPROOF CONCRETE BASED ON FIRE GLASS WITH A LOW IRON CONTENT, SUPPLIED DRY, TYPE OF BOND HYDRAULIC, CHEMICAL COMPOSITION AL2O3 24-28%, SIO2 59-63%, FE2O3 LESS THAN 1.5%. MAXIMUM APPLICATION TEMPERATURE 1200░C. SUPPLIED FOR YOUR OWN | 7000 | 5027.74 | Spain | GORNAL SPAIN | BRANCH OF HAYDELBERGCEMENT RUS LLC ON ORDER OF HAYDELBERGCEMENT RUS LLC |
1/29/2022 | 3816000000 | FIREPROOF CONCRETE BASED ON FIRE GLASS WITH A LOW IRON CONTENT, SUPPLIED DRY, TYPE OF BOND HYDRAULIC, CHEMICAL COMPOSITION AL2O3 24-28%, SIO2 59-63%, FE2O3 LESS THAN 1.5%. MAXIMUM APPLICATION TEMPERATURE 1200░C. SUPPLIED FOR YOUR OWN | 20000 | 14359.5 | Spain | GORNAL SPAIN | BRANCH OF HAYDELBERGCEMENT RUS LLC ON ORDER OF HAYDELBERGCEMENT RUS LLC |